Low-Temperature Luminescence Spectroscopy of Violet Sr-Al-O:Eu2+ Phosphor Particles

Violet Sr–Al–O:Eu2+ phosphor particles were synthesized from a metal–ethylenediaminetetraacetic acid (EDTA) solution of Sr, Al, Eu, and particulate alumina via spray drying and sintering in a reducing atmosphere. The crystal structures and emission properties at 85–300 K were investigated. The composition of the violet Sr–Al–O:Eu2+ phosphor particles was determined from various Sr–Al–O:Eu2+ phosphors by their emission properties’ dependence on temperature. The highly crystalline SrAl12O19:Eu2+ emission phases were confirmed by their crystallite sizes and the activation energies for the 4f5d–8S7/2 transition of the Eu2+ ion. These results showed that the material identification for the violet Sr–Al–O:Eu2+ phosphor was accomplished by the low-temperature luminescence measurements.

Two-Photon Fluorescence in N-Doped Graphene Quantum Dots

Nitrogen-doped graphene quantum dots (N-GQDs) were fabricated by microwave-assisted hydrothermal technique. The optical properties of the N-GQDs were studied. The luminescence of the N-GQDs can be tuned by varying the excitation wavelength. Furthermore, two-photon luminescence of the N-GQDs excited by near-infrared laser can be obtained. It is shown that N-doping play a key role on two-photon luminescence. The N-GQDs are expected to find application in biological applications including bioimaging and sensing.

Effect of Cr and Fe Doping on the Structural and Optical Properties of ZnO Nanostructures

In the present study, we have synthesized Cr and Fe doped zinc oxide (ZnO) nanostructures (Zn1-δCraFebO; where δ = a + b = 20%, a = 5, 6, 8 & 10% and b = 15, 14, 12 & 10%) via sol-gel method at different doping concentrations. The synthesized samples were characterized for structural properties by X-ray diffractrometer and field emission scanning electron microscope and the optical properties were carried out through photoluminescence and UVvisible spectroscopy. The particle size calculated through field emission scanning electron microscope varies from 41 to 96 nm for the samples synthesized at different doping concentrations. The optical band gaps calculated through UV-visible spectroscopy are found to be decreasing from 3.27 to 3.02 eV as the doping concentration of Cr increases and Fe decreases.

Silver Nanoparticles-Enhanced Luminescence Spectra of Silicon Nanocrystals

Metal-enhanced Luminescence of silicon nanocrystals (SiNCs) was determined using two different particle sizes of silver nanoparticles (AgNPs). SiNCs have been characterized by scanning electron microscopy (SEM), high resolution transmission electron microscopy (HRTEM), Fourier transform infrared spectroscopy (FTIR) and X-ray photoelectron spectroscopy (XPS). It is found that the SiNCs are crystalline with an average diameter of 65 nm and FCC lattice. AgNPs were synthesized using photochemical reduction of AgNO3 with sodium dodecyl sulphate (SDS). The enhanced luminescence of SiNCs by AgNPs was evaluated by confocal Raman microspectroscopy. Enhancement up to x9 and x3 times were observed for SiNCs that mixed with AgNPs which have an average particle size of 100 nm and 30 nm, respectively. Silver NPs-enhanced luminescence of SiNCs occurs as a result of the coupling between the excitation laser light and the plasmon bands of AgNPs; thus this intense field at AgNPs surface couples strongly to SiNCs.

Light Emission Enhancement of Silicon Nanocrystals by Gold Layer

A thin gold metal layer was deposited on the top of silicon oxide films containing embedded Si nanocrystals (Si-nc). The sample was annealed in a gas containing nitrogen, and subsequently characterized by photoluminescence. We obtained 3-fold enhancement of photon emission from the Si-nc embedded in silicon dioxide covered with a Gold layer as compared with an uncovered sample. We attribute this enhancement to the increase of the spontaneous emission rate caused by the coupling of the Si-nc emitters with the surface plasmons (SP). The evolution of PL emission with laser irradiated time was also collected from covered samples, and compared to that from uncovered samples. In an uncovered sample, the PL intensity decreases with time, approximately with two decay constants. Although the decrease of the initial PL intensity associated with the increase of sample temperature under CW pumping is still observed in samples covered with a gold layer, this film significantly contributes to reduce the permanent deterioration of the PL intensity. The resistance to degradation of light-emitting silicon nanocrystals can be increased by SP coupling to suppress the permanent deterioration. Controlling the permanent photodeterioration can allow to perform a reliable optical gain measurement.

Metal-Semiconductor-Metal Photodetector Based On Porous In0.08Ga0.92N

Characteristics of MSM photodetector based on a porous In0.08Ga0.92N thin film were reported. Nanoporous structures of n-type In0.08Ga0.92N/AlN/Si thin films were synthesized by photoelectrochemical (PEC) etching at a ratio of 1:4 of HF:C2H5OH solution for 15min. The structural and optical properties of pre- and post-etched thin films were investigated. Field emission scanning electron microscope and atomic force microscope images showed that the pre-etched thin film has a sufficiently smooth surface over a large region and the roughness increased for porous film. Blue shift has been observed in photoluminescence emission peak at 300 K for porous sample. The photoluminescence intensity of the porous film indicated that the optical properties have been enhanced. A high work function metals (Pt and Ni) were deposited as a metal contact on the porous films. The rise and recovery times of the devices were investigated at 390nm chopped light. Finally, the sensitivity and quantum efficiency were also studied.

Portable Continuous Aerosol Concentrator for the Determination of NO2 in the Air

The paper deals with the development of portable aerosol concentrator and its application for the determination of nitrites and nitrates. The device enables the continuous trapping of pollutants in the air. An extensive literature search has been elaborated which aims at the development of samplers and the possibilities of their application in the continuous determination of volatile organic compounds. The practical part of the paper is focused on the development of the portable aerosol concentrator. The device using the Aerosol Enrichment Unit has been experimentally verified and subsequently realized. It operates on the principle of equilibrium accumulation of pollutants from the gaseous phase using absorption liquid polydisperse aerosol. The device has been applied for monitoring nitrites and nitrates in the air. The chemiluminescence detector was used for detection; the achieved detection limit for nitrites was 28 ng/m3 and for nitrates 78 ng/m3.

Surface Morphology and Formation of Nanostructured Porous GaN by UV-assisted Electrochemical Etching

This article reports on the studies of porous GaN prepared by ultra-violet (UV) assisted electrochemical etching in a solution of 4:1:1 HF: CH3OH:H2O2 under illumination of an UV lamp with 500 W power for 10, 25 and 35 minutes. The optical properties of porous GaN sample were compared to the corresponding as grown GaN. Porosity induced photoluminescence (PL) intensity enhancement was found in these samples. The resulting porous GaN displays blue shifted PL spectra compared to the as-grown GaN. Appearance of the blue shifted emission is correlated with the development of highly anisotropic structures in the morphology. An estimate of the size of the GaN nanostructure can be obtained with the help of a quantized state effective mass theory.

Functional Sample of the Portable Device for Fast Analysis of Explosives

The construction of original functional sample of the portable device for fast analysis of energetic materials has been described in the paper. The portable device consisting of two parts – an original miniaturized microcolumn liquid chromatograph and a unique chemiluminescence detector – has been proposed and realized. In a very short time, this portable device is capable of identifying selectively most of military nitramine- and nitroesterbased explosives as well as inorganic nitrates occurring in trace concentrations in water or in soil. The total time required for the identification of extracts is shorter than 8 minutes.

Investigation on Toxicity of Manufactured Nanoparticles to Bioluminescence Bacteria Vibrio fischeri

Acute toxicity of nano SiO2, ZnO, MCM-41 (Meso pore silica), Cu, Multi Wall Carbon Nano Tube (MWCNT), Single Wall Carbon Nano Tube (SWCNT) , Fe (Coated) to bacteria Vibrio fischeri using a homemade luminometer , was evaluated. The values of the nominal effective concentrations (EC), causing 20% and 50% inhibition of biouminescence, using two mathematical models at two times of 5 and 30 minutes were calculated. Luminometer was designed with Photomultiplier (PMT) detector. Luminol chemiluminescence reaction was carried out for the calibration graph. In the linear calibration range, the correlation coefficients and coefficient of Variation (CV) were 0.988 and 3.21% respectively which demonstrate the accuracy and reproducibility of the instrument that are suitable. The important part of this research depends on how to optimize the best condition for maximum bioluminescence. The culture of Vibrio fischeri with optimal conditions in liquid media, were stirring at 120 rpm at a temperature of 150C to 180C and were incubated for 24 to 72 hours while solid medium was held at 180C and for 48 hours. Suspension of nanoparticles ZnO, after 30 min contact time to bacteria Vibrio fischeri, showed the highest toxicity while SiO2 nanoparticles showed the lowest toxicity. After 5 min exposure time, the toxicity of ZnO was the strongest and MCM-41 was the weakest toxicant component.

Photodegradation of Optically Trapped Polystyrene Beads at 442 nm

Polystyrene particles of different sizes are optically trapped with a gaussian beam from a He-Cd laser operating at 442 nm. The particles are observed to exhibit luminescence after a certain trapping time followed by an escape from the optical trap. The observed luminescence is explained in terms of the photodegradation of the polystyrene backbone. It is speculated that these chemical modifications also play a role for the escape of the particles from the trap. Variations of the particle size and the laser power show that these parameters have a great influence on the observed phenomena.

High Optical Properties and Rectifying Behavior of ZnO (Nano and Microstructures)/Si Heterostructures

We investigated a modified thermal evaporation method in the growth process of ZnO nanowires. ZnO nanowires were fabricated on p-type silicon substrates without using a metal catalyst. A simple horizontal double-tube system along with chemical vapor diffusion of the precursor was used to grow the ZnO nanowires. The substrates were placed in different temperature zones, and ZnO nanowires with different diameters were obtained for the different substrate temperatures. In addition to the nanowires, ZnO microdiscs with different diameters were obtained on another substrate, which was placed at a lower temperature than the other substrates. The optical properties and crystalline quality of the ZnO nanowires and microdiscs were characterized by room temperature photoluminescence (PL) and Raman spectrometers. The PL and Raman studies demonstrated that the ZnO nanowires and microdiscs grown using such set-up had good crystallinity with excellent optical properties. Rectifying behavior of ZnO/Si heterostructures was characterized by a simple DC circuit.

Study the Influence of Chemical Treatment on the Compositional Changes and Defect Structures of ZnS Thin Film

The effect of chemical treatment in CdCl2 on the compositional changes and defect structures of potentially useful ZnS solar cell thin films prepared by vacuum deposition method was studied using the complementary Rutherford backscattering (RBS) and Thermoluminesence (TL) techniques. A series of electron and hole traps are found in the various as deposited samples studied. After treatment, perturbation on the intensity is noted; mobile defect states and charge conversion and/or transfer between defect states are found.

Optical Properties of Some A2BCl4 Type Chlorides

Efficient luminescence is reported for the first time in Eu2+ activated double Chlorides A2BCl4 (A=Alkali metal, B=Alkaline earth element). A simple wet-chemical preparation is described. Emission intensities are comparable to that of the commercial phosphor. Excitation covers near UV region. These phosphors may be useful for applications like solid state lighting, scintillation detectors and X-ray storage using photo-stimulable phosphors.

Highly Efficient White Light-emitting Diodes Based on Layered Quantum Dot-Phosphor Nanocomposites as Converting Materials

This paper reports on the enhanced photoluminescence (PL) of nanocomposites through the layered structuring of phosphor and quantum dot (QD). Green phosphor of Sr2SiO4:Eu, red QDs of CdSe/CdS/CdZnS/ZnS core-multishell, and thermo-curable resin were used for this study. Two kinds of composite (layered and mixed) were prepared, and the schemes for optical energy transfer between QD and phosphor were suggested and investigated based on PL decay characteristics. It was found that the layered structure is more effective than the mixed one in the respects of PL intensity, PL decay and thermal loss. When this layered nanocomposite (QDs on phosphor) is used to make white light emitting diode (LED), the brightness is increased by 37 %, and the color rendering index (CRI) value is raised to 88.4 compared to the mixed case of 80.4.

Toxicity Study of Two Different Synthesized Silver Nanoparticles on Bacteria Vibrio Fischeri

A comparative evaluation of acute toxicity of synthesized nano silvers using two different procedures (biological and chemical reduction methods) and silver ions on bacteria Vibrio fischeri was investigated. The bacterial light inhibition test as a toxicological endpoint was used by applying of a homemade luminometer. To compare the toxicity effects as a quantitative parameter, a nominal effective concentrations (EC) of chemicals and a susceptibility constant (Z-value) of bacteria, after 5 min and 30 min exposure times, were calculated. After 5 and 30 min contact times, the EC50 values of two silver nanoparticles and the EC20 values were about similar. It demonstrates that toxicity of silvers was independent of their procedure. The EC values of nanoparticles were larger than those of the silver ions. The susceptibilities(Z- Values) of V.fischeri (L/mg) to the silver ions were greater than those of the nano silvers. According to the EC and Z values, the toxicity of silvers decreased in the following order: Silver ions >> silver nanoparticles from chemical reduction method ~ silver nanoparticles from biological method.

Structural and Optical Properties ofInxAlyGa1-x-yN Quaternary Alloys

Quaternary InxAlyGa1-x-yN semiconductors have attracted much research interest because the use of this quaternary offer the great flexibility in tailoring their band gap profile while maintaining their lattice-matching and structural integrity. The structural and optical properties of InxAlyGa1-x-yN alloys grown by molecular beam epitaxy (MBE) is presented. The structural quality of InxAlyGa1-x-yN layers was characterized using high-resolution X-ray diffraction (HRXRD). The results confirm that the InxAlyGa1-x-yN films had wurtzite structure and without phase separation. As the In composition increases, the Bragg angle of the (0002) InxAlyGa1-x-yN peak gradually decreases, indicating the increase in the lattice constant c of the alloys. FWHM of (0002) InxAlyGa1-x-yN decreases with increasing In composition from 0 to 0.04, that could indicate the decrease of quality of the samples due to point defects leading to non-uniformity of the epilayers. UV-VIS spectroscopy have been used to study the energy band gap of InxAlyGa1-x-yN. As the indium (In) compositions increases, the energy band gap decreases. However, for InxAlyGa1-x-yN with In composition of 0.1, the band gap shows a sudden increase in energy. This is probably due to local alloy compositional fluctuations in the epilayer. The bowing parameter which appears also to be very sensitive on In content is investigated and obtained b = 50.08 for quaternary InxAlyGa1-x-yN alloys. From photoluminescence (PL) measurement, green luminescence (GL) appears at PL spectrum of InxAlyGa1-x-yN, emitted for all x at ~530 nm and it become more pronounced as the In composition (x) increased, which is believed cause by gallium vacancies and related to isolated native defects.

Improvement of Photoluminescence Uniformity of Porous Silicon by using Stirring Anodization Process

The electrolyte stirring method of anodization etching process for manufacturing porous silicon (PS) is reported in this work. Two experimental setups of nature air stirring (PS-ASM) and electrolyte stirring (PS-ESM) are employed to clarify the influence of stirring mechanisms on electrochemical etching process. Compared to traditional fabrication without any stirring apparatus (PS-TM), a large plateau region of PS surface structure is obtained from samples with both stirring methods by the 3D-profiler measurement. Moreover, the light emission response is also improved by both proposed electrolyte stirring methods due to the cycling force in electrolyte could effectively enhance etch-carrier distribution while the electrochemical etching process is made. According to the analysis of statistical calculation of photoluminescence (PL) intensity, lower standard deviations are obtained from PS-samples with studied stirring methods, i.e. the uniformity of PL-intensity is effectively improved. The calculated deviations of PL-intensity are 93.2, 74.5 and 64, respectively, for PS-TM, PS-ASM and PS-ESM.

Facile Synthesis of Vertically Aligned ZnO Nanowires on Carbon Layer by Vapour Deposition

A facile vapour deposition method of synthesis of vertically aligned ZnO nanowires on carbon seed layer was developed. The received samples were investigated on electronic microscope JSM-6490 LA JEOL and x-ray diffractometer X, pert MPD PRO. The photoluminescence spectra (PL) of obtained ZnO samples at a room temperature were studied using He-Cd laser (325 nm line) as excitation source.

Synthesis, Characterization and PL Properties of Cds Nanoparticles Confined within a Functionalized SBA-15 Mesoprous

A simple and dexterous in situ method was introduced to load CdS nanocrystals into organofunctionalized mesoporous, which used an ion-exchange method. The products were extensively characterized by combined spectroscopic methods. X- ray diffraction (XRD) and high-resolution transmission electron microscopy (HRTEM) demonstrated both the maintenance of pore symmetry (space group p6mm) of SBA-15 and the presence of CdS nanocrystals with uniform sizes of about 6 - 8 nm inside the functionalized SBA-15 channels. These mesoporous silica-supported CdS composites showed room temperature photoluminescence properties with a blue shift, indicating the quantum size effect of nanocrystalline CdS.