Abstract: Microstructure analysis of additively manufactured (AM) materials is an important step in understanding the interrelationship between mechanical properties and materials performance. Literature on the effect of a laser-based AM process parameters on the microstructure in the substrate-deposit interface is limited. The interface region, the adjoining area of substrate and deposit, is characterized by the presence of the fusion zone (FZ) and heat affected zone (HAZ) experiencing rapid thermal gyrations resulting in thermal induced transformations. Inconel 718 was utilized as a work material for both the substrate and deposit. Three blocks of Inconel 718 material were deposited by Direct Energy Deposition (DED) using three different laser powers, 550W, 750W and 950W, respectively. A coupled thermo-mechanical transient approach was utilized to correlate temperature history to the evolution of microstructure. Thermal history of the deposition process was monitored with the thermocouples installed inside the substrate material. Interface region of the blocks were analysed with Optical Microscopy (OM) and Scanning Electron Microscopy (SEM) including electron back-scattered diffraction (EBSD) technique. Laser power was found to influence the dissolution of intermetallic precipitated phases in the substrate and grain growth in the interface region. Microstructure and thermal history data were utilized to draw conclusive comparisons between the investigated process parameters.
Abstract: The major concern in the aviation industry is the flight safety. Although great effort has been put onto the development of material and system reliability, the failure cases of fatal accidents still occur nowadays. Due to the complexity of the aviation system, and the interaction among the failure components, the failure analysis of the related equipment is a little difficult. This study focuses on surveying the failure cases in aviation, which are extracted from failure analysis journals, including Engineering Failure Analysis and Case studies in Engineering Failure Analysis, in order to obtain the failure sensitive factors or failure sensitive parts. The analytical results show that, among the failure cases, fatigue failure is the largest in number of occurrence. The most failed components are the disk, blade, landing gear, bearing, and fastener. The frequently failed materials consist of steel, aluminum alloy, superalloy, and titanium alloy. Therefore, in order to assure the safety in aviation, more attention should be paid to the fatigue failures.
Abstract: Nickel-based superalloys are generally known to be difficult to cut due to their strength, low thermal conductivity, and high work hardening tendency. Superalloy such as alloy 625 is often used in the oil and gas industry as a surfacing material to provide wear and corrosion resistance to components. The material is typically applied onto a metallic substrate through weld overlay cladding, an arc welding technique. Cladded surfaces are always rugged and carry a tough skin; this creates further difficulties to the machining process. The present work utilised design of experiment to optimise the internal cylindrical rough turning for weld overlay surfaces. An L27 orthogonal array was used to assess effects of the four selected key process variables: cutting insert, depth of cut, feed rate, and cutting speed. The optimal cutting conditions were determined based on productivity and the level of tool wear.
Abstract: Cutting tools with ceramic inserts are often used in the process of machining many types of superalloy, mainly due to their high strength and thermal resistance. Nevertheless, during the cutting process, the plastic flow wear generated in these inserts enhances and propagates cracks due to high temperature and high mechanical stress. This leads to a very variable failure of the cutting tool. This article explores the relationship between the continuous wear that ceramic SiAlON (solid solutions based on the Si3N4 structure) inserts experience during a high-speed machining process and the evolution of sparks created during the same process. These sparks were analysed through pictures of the cutting process recorded using an SLR camera. Features relating to the intensity and area of the cutting sparks were extracted from the individual pictures using image processing techniques. These features were then related to the ceramic insert’s crater wear area.
Abstract: In this study, nickel aluminide coatings were deposited onto CMSX-4 single crystal superalloy and pure Ni substrates by using in-situ chemical vapour deposition (CVD) technique. The microstructural evolutions and coating thickness (CT) were studied upon the variation of processing conditions i.e. time and temperature. The results demonstrated (under identical conditions) that coating formed on pure Ni contains no substrate entrapments and have lower CT in comparison to one deposited on the CMSX-4 counterpart. In addition, the interdiffusion zone (IDZ) of Ni substrate is a γ’-Ni3Al in comparison to the CMSX-4 alloy that is βNiAl phase. The higher CT on CMSX-4 superalloy is attributed to presence of γ-Ni/γ’-Ni3Al structure which contains ~ 15 at.% Al before deposition (that is already present in superalloy). Two main deposition parameters (time and temperature) of the coatings were also studied in addition to standard comparison of substrate effects. The coating formation time was found to exhibit profound effect on CT, whilst temperature was found to change coating activities. In addition, the CT showed linear trend from 800 to 1000 °C, thereafter reduction was observed. This was attributed to the change in coating activities.
Abstract: Haynes 25 alloy (also known as L-605 alloy) is cobalt
based super alloy which has widely applications such as aerospace
industry, turbine and furnace parts, power generators and heat
exchangers and petroleum refining components due to its excellent
characteristics. However, the workability of this alloy is more
difficult compared to normal steels or even stainless. In present work,
an experimental investigation was performed under cryogenic
cooling to determine cutting tool wear patterns and obtain optimal
cutting parameters in turning of cobalt based superalloy Haynes 25.
In experiments, uncoated carbide tool was used and cutting speed (V)
and feed rate (f) were considered as test parameters. Tool wear
(VBmax) were measured for process performance indicators.
Analysis of variance (ANOVA) was performed to determine the
importance of machining parameters.
Abstract: High pressure turbine (HPT) blades of DV – 2 jet
engines are made from Ni – based superalloy. This alloy was
originally manufactured in the Soviet Union and referred as ŽS6K.
For improving alloy’s high temperature resistance are blades coated
with Al – Si diffusion layer. A regular operation temperature of HPT
blades vary from 705°C to 750°C depending on jet engine regime.
An overcrossing working temperature range causes degradation of
the protective coating as well as base material which microstructure
is formed by the gamma matrix and strengthening phase gamma
prime (forming small particles in the microstructure). Diffusion
processes inside the material during exposition of the material to high
temperatures causes mainly coarsening of the gamma prime particles,
thus decreasing its strengthening effect. Degradation of the Al – Si
coating caused its thickness growth. All the microstructure changes
and coating layer thickness growth results in decreasing of the turbine
blade operation lifetime.
Abstract: Over the past four decades, the fatigue behavior of
nickel-based alloys has been widely studied. However, in recent
years, significant advances in the fabrication process leading to grain
size reduction have been made in order to improve fatigue properties
of aircraft turbine discs. Indeed, a change in particle size affects the
initiation mode of fatigue cracks as well as the fatigue life of the
material. The present study aims to investigate the fatigue behavior of
a newly developed nickel-based superalloy under biaxial-planar
loading. Low Cycle Fatigue (LCF) tests are performed at different
stress ratios so as to study the influence of the multiaxial stress state
on the fatigue life of the material. Full-field displacement and strain
measurements as well as crack initiation detection are obtained using
Digital Image Correlation (DIC) techniques. The aim of this
presentation is first to provide an in-depth description of both the
experimental set-up and protocol: the multiaxial testing machine, the
specific design of the cruciform specimen and performances of the
DIC code are introduced. Second, results for sixteen specimens
related to different load ratios are presented. Crack detection, strain
amplitude and number of cycles to crack initiation vs. triaxial stress
ratio for each loading case are given. Third, from fractographic
investigations by scanning electron microscopy it is found that the
mechanism of fatigue crack initiation does not depend on the triaxial
stress ratio and that most fatigue cracks initiate from subsurface
carbides.
Abstract: The impact deformation and fracture behaviour of cobalt-based Haynes 188 superalloy are investigated by means of a split Hopkinson pressure bar. Impact tests are performed at strain rates ranging from 1×103 s-1 to 5×103 s-1 and temperatures between 25°C and 800°C. The experimental results indicate that the flow response and fracture characteristics of cobalt-based Haynes 188 superalloy are significantly dependent on the strain rate and temperature. The flow stress, work hardening rate and strain rate sensitivity all increase with increasing strain rate or decreasing temperature. It is shown that the impact response of the Haynes 188 specimens is adequately described by the Zerilli-Armstrong fcc model. The fracture analysis results indicate that the Haynes 188 specimens fail predominantly as the result of intensive localised shearing. Furthermore, it is shown that the flow localisation effect leads to the formation of adiabatic shear bands. The fracture surfaces of the deformed Haynes 188 specimens are characterised by dimple- and / or cleavage-like structure with knobby features. The knobby features are thought to be the result of a rise in the local temperature to a value greater than the melting point.
Abstract: This presentation reviews recent advances in superalloys and thermal barrier coating (TBC) for application in hot sections of energy-efficient gas-turbine engines. It has been reviewed that in the modern combined-cycle gas turbines (CCGT) applying single-crystal energy materials (SC superalloys) and thermal barrier coatings (TBC), and – in one design – closed-loop steam cooling, thermal efficiency can reach more than 60%. These technological advancements contribute to profitable and clean power generation with reduced emission. Alternatively, the use of advanced superalloys (e.g. GTD-111 superalloy, Allvac 718Plus superalloy) and advanced thermal barrier coatings (TBC) in modern gas-turbines has been shown to yield higher energy-efficiency in power generation.