Abstract: In the present study, the incorporation of graphene
into blends of acrylonitrile-butadiene-styrene terpolymer with
polypropylene (ABS/PP) was investigated focusing on the
improvement of their thermomechanical characteristics and the effect
on their rheological behavior. The blends were prepared by melt
mixing in a twin-screw extruder and were characterized by measuring
the MFI as well as by performing DSC, TGA and mechanical tests.
The addition of graphene to ABS/PP blends tends to increase their
melt viscosity, due to the confinement of polymer chains motion.
Also, graphene causes an increment of the crystallization temperature
(Tc), especially in blends with higher PP content, because of the
reduction of surface energy of PP nucleation, which is a consequence
of the attachment of PP chains to the surface of graphene through the
intermolecular CH-π interaction. Moreover, the above nanofiller
improves the thermal stability of PP and increases the residue of
thermal degradation at all the investigated compositions of blends,
due to the thermal isolation effect and the mass transport barrier
effect. Regarding the mechanical properties, the addition of graphene
improves the elastic modulus, because of its intrinsic mechanical
characteristics and its rigidity, and this effect is particularly strong in
the case of pure PP.
Abstract: This paper presents a part of research on the
rheological properties of bitumen modified by thermoplastic namely
linear low density polyethylene (LLDPE), high density polyethylene
(HDPE) and polypropylene (PP) and its interaction with 80 pen base
bitumen. As it is known that the modification of bitumen by the use
of polymers enhances its performance characteristics but at the same
time significantly alters its rheological properties. The rheological
study of polymer modified bitumen (PMB) was made through
penetration, ring & ball softening point and viscosity test. The results
were then related to the changes in the rheological properties of
polymer modified bitumen. It was observed that thermoplastic
copolymer shows profound effect on penetration rather than
softening point. The viscoelastic behavior of polymer modified
bitumen depend on the concentration of polymer, mixing
temperature, mixing technique, solvating power of base bitumen and
molecular structure of polymer used. PP offer better blend in
comparison to HDPE and LLDPE. The viscosity of base bitumen was
also enhanced with the addition of polymer. The pseudoplastic
behavior was more prominent for HDPE and LLDPE than PP. Best
results were obtained when polymer concentration was kept below
3%
Abstract: In this research work, poly (acrylonitrile-butadienestyrene)/
polypropylene (ABS/PP) blends were processed by melt
compounding in a twin-screw extruder. Upgrading of the thermal
characteristics of the obtained materials was attempted by the
incorporation of organically modified montmorillonite (OMMT), as
well as, by the addition of two types of compatibilizers;
polypropylene grafted with maleic anhydride (PP-g-MAH) and ABS
grafted with maleic anhydride (ABS-g-MAH). The effect of the
above treatments was investigated separately and in combination.
Increasing the PP content in ABS matrix seems to increase the
thermal stability of their blend and the glass transition temperature
(Tg) of SAN phase of ABS. From the other part, the addition of ABS
to PP promotes the formation of its β-phase, which is maximum at 30
wt% ABS concentration, and increases the crystallization temperature
(Tc) of PP. In addition, it increases the crystallization rate of PP.The
β-phase of PP in ABS/PP blends is reduced by the addition of
compatibilizers or/and organoclay reinforcement. The incorporation
of compatibilizers increases the thermal stability of PP and reduces
its melting (ΔΗm) and crystallization (ΔΗc) enthalpies. Furthermore it
decreases slightly the Tgs of PP and SAN phases of ABS/PP blends.
Regarding the storage modulus of the ABS/PP blends, it presents a
change in their behavior at about 10°C and return to their initial
behavior at ~110°C. The incorporation of OMMT to no compatibilized
and compatibilized ABS/PP blends enhances their storage modulus.
Abstract: Plastics occupy wide place in the applications of
automotive, electronics and house goods. Especially reinforced
plastics become popular because of their high strength besides their
advantages of low weight and easy manufacturability. In this study,
mechanical and morphological properties of polypropylene (PP) and
high density polyethylene (HDPE) matrix composites reinforced with
surface modified nano titan dioxide (TiO2) particles were
investigated. Surface modification was made by coating the nano
powders with maleic anhydride grafted styrene ethylene butylene
styrene (SEBS-g-MA) and silane, respectively. After surface
modification, PP/TiO2 and HDPE/TiO2 composites were obtained by
using twin screw extruder at titan dioxide loading of 1 wt.%, 3 wt.%
and 5 wt.%. Effects of surface modification were determined by
thermal and morphological analysis. SEBS-g-MA provided bridging
effect between TiO2 particles and polymer matrix while silane was
effective as a dispersant. Depending on that, homogenous structures
without agglomeration were obtained. Mechanical tests were
performed on the injection moldings of the composites for obtaining
the impact strength, tensile strength, stress at break, elongation and
elastic modulus. Reinforced HDPE and PP moldings gave higher
tensile strength and elastic modulus due to the rigid structure of TiO2.
Slight increment was seen in stress at break. Elongation and impact
strength decreased due to the stiffness of the nano titan dioxide.
Abstract: Low silica type X (LSX) Zeolite is one of useful
material in many manufacturing due to the advantage properties
including high surface area, stability, microporous crystalline
aluminosilicates and positive ion in an extra–framework. The LSX
was used rice husk silica source which obtained by leaching with
hydrochloric acid and calcination at 500C. To improve the
synthesis method, the LSX was crystallizated in Teflon–lined
autoclave will expedite deceasing of the amorphous particles. The
mixed gel with composition of 5.5 Na2O : 1.65 K2O : Al2O3 : 2.2
SiO2 : 122 H2O was crystallized in different container
(Polypropylene bottom and Teflon–lined autoclave). The obtained
powder was characterized by X–ray diffraction (XRD), X–ray
fluorescence spectrometry, N2 adsorption-desorption analysis BET
surface area Scanning electron microscopy (SEM) and Fourier
transform infrared spectroscopy to justify the quality of zeolite. The
results showed the crystallized zeolite in Teflon lined autoclave has
102.8 nm of crystal size, 286 m2/g of surface area and fewer amounts
of round amorphous particles when compared with the crystallized
zeolite in Polypropylene.
Abstract: Paper presents knowledge about types of test in area
of materials properties of selected methods of rapid prototyping
technologies. In today used rapid prototyping technologies for
production of models and final parts are used materials in initial state
as solid, liquid or powder material structure. In solid state are used
various forms such as pellets, wire or laminates. Basic range
materials include paper, nylon, wax, resins, metals and ceramics. In
Fused Deposition Modeling (FDM) rapid prototyping technology are
mainly used as basic materials ABS (Acrylonitrile Butadiene
Styrene), polyamide, polycarbonate, polyethylene and polypropylene.
For advanced FDM applications are used special materials as silicon
nitrate, PZT (Piezoceramic Material - Lead Zirconate Titanate),
aluminium oxide, hydroxypatite and stainless steel.