Abstract: In order to produce lead free piezoceramics with
optimum piezoelectric and dielectric properties, KNN modified with
Li+ (as an A site dopant) and Sb5+ (as a B site dopant)
(K0.49Na0.49Li0.02) (Nb0.96Sb0.04) O3 (referred as KNLNS in this paper)
have been synthesized using solid state reaction method and
conventional sintering technique. The ceramics were sintered in the
narrow range of 1050°C-1090°C for 2-3 h to get precise information
about sintering parameters. Detailed study of dependence of
microstructural, dielectric and piezoelectric properties on sintering
conditions was then carried out. The study suggests that the volatility
of the highly hygroscopic KNN ceramics is not only sensitive to
sintering temperatures but also to sintering durations. By merely
reducing the sintering duration for a given sintering temperature we
saw an increase in the density of the samples which was supported by
the increase in dielectric constants of the ceramics. And since density
directly or indirectly affects almost all the associated properties, other
dielectric and piezoelectric properties were also enhanced as we
approached towards the most suitable sintering temperature and
duration combination. The detailed results are reported in this paper.
Abstract: Nanocrystalline powders of the lead-free piezoelectric
material, tantalum-substituted potassium sodium niobate
(K0.5Na0.5)(Nb0.9Ta0.1)O3 (KNNT), were produced using a Retsch
PM100 planetary ball mill by setting the milling time to 15h, 20h,
25h, 30h, 35h and 40h, at a fixed speed of 250rpm. The average
particle size of the milled powders was found to decrease from 12nm
to 3nm as the milling time increases from 15h to 25h, which is in
agreement with the existing theoretical model. An anomalous
increase to 98nm and then a drop to 3nm in the particle size were
observed as the milling time further increases to 30h and 40h
respectively. Various sizes of these starting KNNT powders were
used to investigate the effect of milling time on the microstructure,
dielectric properties, phase transitions and piezoelectric properties of
the resulting KNNT ceramics. The particle size of starting KNNT
was somewhat proportional to the grain size. As the milling time
increases from 15h to 25h, the resulting ceramics exhibit
enhancement in the values of relative density from 94.8% to 95.8%,
room temperature dielectric constant (εRT) from 878 to 1213, and
piezoelectric charge coefficient (d33) from 108pC/N to 128pC/N. For
this range of ceramic samples, grain size refinement suppresses the
maximum dielectric constant (εmax), shifts the Curie temperature (Tc)
to a lower temperature and the orthorhombic-tetragonal phase
transition (Tot) to a higher temperature. Further increase of milling
time from 25h to 40h produces a gradual degradation in the values of
relative density, εRT, and d33 of the resulting ceramics.
Abstract: We propose an unconstrained measurement system for scratching motion based on mathematical model of unconstrained bed sensing method which could measure the bed vibrations due to the motion of the person on the bed. In this paper, we construct mathematical model of the unconstrained bed monitoring system; and we apply the unconstrained bed sensing method to the system for detecting scratching motion. The proposed sensors are placed under the three bed feet. When the person is lying on the bed, the output signals from the sensors are proportional to the magnitude of the vibration due to the scratching motion. Hence, we could detect the subject’s scratching motion from the output signals from ceramic sensors. We evaluated two scratching motions using the proposed system in the validity experiment as follows: 1st experiment is the subject’s scratching the right side cheek with his right hand, and; 2nd experiment is the subject’s scratching the shin with another foot. As the results of the experiment, we recognized the scratching signals that enable the determination when the scratching occurred. Furthermore, the difference among the amplitudes of the output signals enabled us to estimate where the subject scratched.
Abstract: This paper presents an exact solution and a finite element method (FEM) for a Piezoceramic Rod under static load. The cylindrical rod is made from polarized ceramics (piezoceramics) with axial poling. The lateral surface of the rod is traction-free and is unelectroded. The two end faces are under a uniform normal traction. Electrically, the two end faces are electroded with a circuit between the electrodes, which can be switched on or off. Two cases of open and shorted electrodes (short circuit and open circuit) will be considered. Finally, a finite element model will be used to compare the results with an exact solution. The study uses ABAQUS (v.6.7) software to derive the finite element model of the ceramic rod.