Monitoring CO2 and H2S Emission in Live Austrian and UK Concrete Sewer Pipes

Corrosion of concrete sewer pipes induced by sulfuric acid is an acknowledged problem and a ticking time-bomb to sewer operators. Whilst the chemical reaction of the corrosion process is well-understood, the indirect roles of other parameters in the corrosion process which are found in sewer environment are not highly reflected on. This paper reports on a field studies undertaken in Austria and United Kingdom, where the parameters of temperature, pH, H2S and CO2 were monitored over a period of time. The study establishes that (i) effluent temperature and pH have similar daily pattern and peak times, when examined in minutes scale; (ii) H2S and CO2 have an identical hourly pattern; (iii) H2S instant or shifted relation to effluent temperature is governed by the root mean square value of CO2.