Abstract: The paper deals with the problems of the actual
behavior, failure mechanism and load-carrying capacity of the special
bolt connection developed and intended for the assembly connections
of truss main girders of perspective railway temporary steel bridges.
Within the framework of this problem solution, several types of
structural details of assembly joints have been considered as the
conceptual structural design. Based on the preliminary evaluation of
advantages or disadvantages of these ones, in principle two basic
structural configurations – so-called “tooth” and “splice-plate”
connections have been selected for the subsequent detailed
investigation. This investigation is mainly based on the experimental
verification of the actual behavior, strain and failure mechanism and
corresponding strength of the connection, and on its numerical
modeling using FEM. This paper is focused only on the cyclic
loading (fatigue) tests results of “splice-plate” connections and their
evaluation, which have already been finished. Simultaneously with
the fatigue tests, the static loading tests have been realized too, but
these ones, as well as FEM numerical modeling, are not the subject of
this paper.
Abstract: Dual phase steels (DPS)s have a microstructure
consisting of a hard second phase called Martensite in the soft Ferrite
matrix. In recent years, there has been interest in dual-phase steels,
because the application of these materials has made significant usage;
particularly in the automotive sector Composite microstructure of
(DPS)s exhibit interesting characteristic mechanical properties such
as continuous yielding, low yield stress to tensile strength
ratios(YS/UTS), and relatively high formability; which offer
advantages compared with conventional high strength low alloy
steels(HSLAS). The research dealt with the characterization of
damage in (DPS)s. In this study by review the mechanisms of failure
due to volume fraction of martensite second phase; a new method is
introduced to identifying the mechanisms of failure in the various
phases of these types of steels. In this method the acoustic emission
(AE) technique was used to detect damage progression. These failure
mechanisms consist of Ferrite-Martensite interface decohesion and/or
martensite phase fracture. For this aim, dual phase steels with
different volume fraction of martensite second phase has provided by
various heat treatment methods on a low carbon steel (0.1% C), and
then AE monitoring is used during tensile test of these DPSs. From
AE measurements and an energy ratio curve elaborated from the
value of AE energy (it was obtained as the ratio between the strain
energy to the acoustic energy), that allows detecting important
events, corresponding to the sudden drops. These AE signals events
associated with various failure mechanisms are classified for ferrite
and (DPS)s with various amount of Vm and different martensite
morphology. It is found that AE energy increase with increasing Vm.
This increasing of AE energy is because of more contribution of
martensite fracture in the failure of samples with higher Vm. Final
results show a good relationship between the AE signals and the
mechanisms of failure.