Abstract: The fly ash of waste incineration processes is usually hazardous and the disposal or reuse of waste incineration fly ash is difficult. In this study, the waste incineration fly ash was converted to useful zeolites by the alkali fusion and hydrothermal synthesis method. The influence of different operating conditions (the ratio of Si/Al, the ratio of hydrolysis liquid to solid, and hydrothermal time) was investigated to seek the optimum operating conditions for the synthesis of zeolite from waste incineration fly ash. The results showed that concentrations of heavy metals in the leachate of Toxicity Characteristic Leaching Procedure (TCLP) were all lower than the regulatory limits except lead. The optimum operating conditions for the synthesis of zeolite from waste incineration fly ash by the alkali fusion and hydrothermal synthesis method were Si/Al=40, NaOH/ash=1.5, alkali fusion at 400 oC for 40 min, hydrolysis with Liquid to Solid ratio (L/S)= 200 at 105 oC for 24 h, and hydrothermal synthesis at 105 oC for 24 h. The specific surface area of fly ash could be significantly increased from 8.59 m2/g to 651.51 m2/g (synthesized zeolite). The influence of different operating conditions on the synthesis of zeolite from waste incineration fly ash followed the sequence of Si/Al ratio > hydrothermal time > hydrolysis L/S ratio. The synthesized zeolites can be reused as good adsorbents to control the air or wastewater pollutants. The purpose of fly ash detoxification, reduction and waste recycling/reuse is achieved successfully.
Abstract: Coal fly ash is formed as a solid waste product from
the combustion of coal in coal fired power stations. Huge amounts of
fly ash are produced globally every year and are predicted to
increase. Nowadays, less than half of the fly ash is used as a raw
material for cement manufacturing, construction and the rest of it is
disposed as a waste causing yet another environmental concern. For
this reason, the recycling of this kind of slurries into useful materials
is quite important in terms of economical and environmental aspects.
The purpose of this study is to evaluate the Orhaneli and
Tuncbilek coal fly ashes for utilization in some industrial
applications. Therefore the mineralogical and chemical compositions
of these fly ashes were analyzed by X-ray fluorescence spectroscopy,
ourier-transform infrared spectrometer, and X-ray diffraction. The
silicon (Si) and aluminum (Al) in the fly ashes were activated by
alkali fusion technique with sodium hydroxide. The obtained extracts
were analyzed for Si and Al content by inductively coupled plasma
optical emission spectrometry.
Abstract: Silica was extracted from agriculture waste rice husk
ash (RHA) and was used as the silica source for synthesis of
RMCM-48 and RSBA-16. An alkali fusion process was utilized to
separate silicate supernatant and the sediment effectively. The
CTAB/Si and F127/Si molar ratio was employed to control the
structure properties of the obtained RMCM-48 and RSBA-16
materials. The N2 adsorption-desorption results showed the
micro-mesoporous RSBA-16 possessed high specific surface areas
(662-1001 m2/g). All the obtained RSBA-16 materials were applied as
the adsorbents for acetone adsorption. And the breakthrough tests
clearly revealed that the RSBA-16(0.004) materials could achieve the
highest acetone adsorption capacity of 181 mg/g under 1000 ppmv
acetone vapor concentration at 25oC, which was also superior to
ZSM-5 (71mg/g) and MCM-41 (157mg/g) under same test conditions.
This can help to reduce the solid waste and the high adsorption
performance of the obtained materials could consider as potential
adsorbents for acetone adsorption.