Abstract: Since columns are the most important elements of the
structures, failure of one column in a critical location can cause a
progressive collapse. In this respect, the repair and strengthening of
columns is a very important subject to reduce the building failure and
to keep the columns capacity. Twenty columns with different
parameters is tested and analysis. Eleven typical confined reinforced
concrete (RC) columns with different types of techniques are
assessment. And also, four confined concrete columns with plastic
tube (PVC) are tested with and with four paralleling tested of
unconfined plain concrete. The techniques of confined RC columns
are mortar strengthening, Steel rings strengthening, FRP
strengthening. Moreover, the technique of confined plain concrete
(PC) column is used PVC tubes. The columns are tested under
uniaxial compressive loads studied the effect of confinement on the
structural behavior of circular RC columns. Test results for each
column are presented in the form of crack patterns, stress-strain
curves. Test results show that confining of the RC columns using
different techniques of strengthening results significant improvement
of the general behavior of the columns and can used in construction.
And also, tested confined PC columns with PVC tubes results shown
that the confined PC with PVC tubes can be used in economical
building. The theoretical model for predicted column capacity is
founded with experimental factor depends on the confined techniques
used and the strain reduction.
Abstract: The main objective of this paper is study the influence
of carbon nano-tubes fibers and nano silica fibers on the
characteristic compressive strength and flexural strength on concrete
and cement mortar. Twelve tested specimens were tested with square
section its dimensions (4040 160) mm, divided into four groups.
The first and second group studied the effect of carbon nano-tubes
(CNTs) fibers with different percentage equal to 0.0, 0.11%, 0.22%,
and 0.33% by weight of cement and effect of nano-silica (nS) fibers
with different percentages equal to 0.0, 1.0%, 2.0%, and 3.0% by
weight of cement on the cement mortar. The third and fourth groups
studied the effect of CNTs fiber with different percentage equal to
0.0%, 0.11%, and 0.22% by weight of cement, and effect of nS fibers
with different percentages were equal to 0.0%, 1.0%, and 2.0% by
weight of cement on the concrete. The compressive strength and
flexural strength at 7, 28, and 90 days is determined. From analysis of
tested results concluded that the nano-fibers is more effective when
used with cement mortar more than used with concrete because of
increasing the surface area, decreasing the pore and the collection of
nano-fibers. And also by adding nano-fibers the improvement of
flexural strength of concrete and cement mortar is more than
improvement of compressive strength.