Abstract: This work aims to investigate the properties and microstructure of diamond-like carbon film deposited by pulsed laser deposition by ablation of a graphite target in a vacuum chamber on a steel substrate. The equipment was mounted to provide one laser beam. The target of high purity graphite and the steel substrate were polished. The mechanical and tribological properties of the film were characterized using Raman spectroscopy, nanoindentation test, scratch test, roughness profile, tribometer, optical microscopy and SEM images. It was concluded that the pulsed laser deposition (PLD) technique associated with the low-pressure chamber and a graphite target provides a good fraction of sp3 bonding, that the process variable as surface polishing and laser parameter have great influence in tribological properties and in adherence tests performance. The optical microscopy images are efficient to identify the metallurgical bond.
Abstract: Fe-based amorphous feedstock powders are used as the matrix into which various ratios of hard B4C nanoparticles (0, 5, 10, 15, 20 vol.%) as reinforcing agents were prepared using a planetary high-energy mechanical milling. The ball-milled nanocomposite feedstock powders were also sprayed by means of high-velocity oxygen fuel (HVOF) technique. The characteristics of the powder particles and the prepared coating depending on their microstructures and nanohardness were examined in detail using nanoindentation tester. The results showed that the formation of the Fe-based amorphous phase was noticed over the course of high-energy ball milling. It is interesting to note that the nanocomposite coating is divided into two regions, namely, a full amorphous phase region and homogeneous dispersion of B4C nanoparticles with a scale of 10–50 nm in a residual amorphous matrix. As the B4C content increases, the nanohardness of the composite coatings increases, but the fracture toughness begins to decrease at the B4C content higher than 20 vol.%. The optimal mechanical properties are obtained with 15 vol.% B4C due to the suitable content and uniform distribution of nanoparticles. Consequently, the changes in mechanical properties of the coatings were attributed to the changes in the brittle to ductile transition by adding B4C nanoparticles.
Abstract: Nitrogen implantation in aluminum and its alloys is acquainted for the difficulties in obtaining modified layers deeper than 200 nm. The present work addresses a new method to overcome such a problem; although, the coating with nitrogen and oxygen obtained by plasma immersion ion implantation (PIII) into a 7075 aluminum alloy surface was too shallow. This alloy is commonly used for structural parts in aerospace applications. Such a layer was characterized by secondary ion mass spectroscopy, electron microscopy, and nanoindentation experiments reciprocating wear tests. From the results, one can assume that the wear of this aluminum alloy starts presenting severe abrasive wear followed by an additional adhesive mechanism. PIII produced a slight difference, as shown in all characterizations carried out in this work. The results shown here can be used as the scientific basis for further nitrogen PIII experiments in aluminum alloys which have the goal to produce thicker modified layers or to improve their surface properties.
Abstract: An ion implantation technique was used for designing the surface area of a titanium alloy and for irradiation-enhanced hardening of the surface. The Ti6Al4V alloy was treated by nitrogen ion implantation at fluences of 2·1017 and 4·1017 cm-2 and at ion energy 90 keV. The depth distribution of the nitrogen was investigated by Rutherford Backscattering Spectroscopy. The gradient of mechanical properties was investigated by nanoindentation. The continuous measurement mode was used to obtain depth profiles of the indentation hardness and the reduced storage modulus of the modified surface area. The reduced storage modulus and the hardness increase with increasing fluence. Increased fluence shifts the peak of the mechanical properties as well as the peak of nitrogen concentration towards to the surface. This effect suggests a direct relationship between mechanical properties and nitrogen distribution.
Abstract: Graphene, a single-atom sheet, has been considered as
the most promising material for making future nanoelectromechanical
systems as well as purely electrical switching with graphene
transistors. Graphene-based devices have advantages in scaled-up
device fabrication due to the recent progress in large area graphene
growth and lithographic patterning of graphene nanostructures. Here
we investigated its mechanical responses of circular graphene
nanoflake under the nanoindentation using classical molecular
dynamics simulations. A correlation between the load and the
indentation depth was constructed. The nanoindented force in this
work was applied to the center point of the circular graphene nanoflake
and then, the resonance frequency could be tuned by a nanoindented
depth. We found the hardening or the softening of the graphene
nanoflake during its nanoindented-deflections, and such properties
were recognized by the shift of the resonance frequency. The
calculated mechanical parameters in the force-vs-deflection plot were
in good agreement with previous experimental and theoretical works.
This proposed schematics can detect the pressure via the deflection
change or/and the resonance frequency shift, and also have great
potential for versatile applications in nanoelectromechanical systems.
Abstract: The present study deals with the characterization of
CrSiN coatings obtained by PVD magnetron sputtering systems.
CrSiN films were deposited with different Si contents, in order to
check the effect of at.% variation on the different properties of the
Cr–N system. Coatings were characterized by scanning electron
microscopy (SEM) for thickness measurements, X-ray diffraction.
Surface morphology and the roughness characteristics were explored
using AFM, Mechanicals properties, elastic and plastic deformation
resistance of thin films were investigated using nanoindentation test. We observed that the Si addition improved the hardness and the
Young’s modulus of the Cr–N system. Indeed, the hardness value is
18,56 GPa for CrSiN coatings. Besides, the Young’s modulus value
is 224,22 GPa for CrSiN coatings for Si content of 1.2 at.%.
Abstract: These Monolayer and multilayer coatings of CrN and
AlCrN deposited on 100Cr6 (AISI 52100) substrate by PVD
magnetron sputtering system. The microstructures of the coatings
were characterized using atomic force microscopy (AFM). The AFM
analysis revealed the presence of domes and craters that are
uniformly distributed over all surfaces of the various layers.
Nanoindentation measurement of CrN coating showed maximum
hardness (H) and modulus (E) of 14 GPa and 190 GPa, respectively.
The measured H and E values of AlCrN coatings were found to be 30
GPa and 382 GPa, respectively. The improved hardness in both the
coatings was attributed mainly to a reduction in crystallite size and
decrease in surface roughness. The incorporation of Al into the CrN
coatings has improved both hardness and Young’s modulus.
Abstract: The nanoindentation behaviour and phase
transformation of annealed single-crystal silicon wafers are examined.
The silicon specimens are annealed at temperatures of 250, 350 and
450ºC, respectively, for 15 minutes and are then indented to maximum
loads of 30, 50 and 70 mN. The phase changes induced in the indented
specimens are observed using transmission electron microscopy
(TEM) and micro-Raman scattering spectroscopy (RSS). For all
annealing temperatures, an elbow feature is observed in the unloading
curve following indentation to a maximum load of 30 mN. Under
higher loads of 50 mN and 70 mN, respectively, the elbow feature is
replaced by a pop-out event. The elbow feature reveals a complete
amorphous phase transformation within the indented zone, whereas
the pop-out event indicates the formation of Si XII and Si III phases.
The experimental results show that the formation of these crystalline
silicon phases increases with an increasing annealing temperature and
indentation load. The hardness and Young’s modulus both decrease as
the annealing temperature and indentation load are increased.
Abstract: Hysitron TriboIndenterTM TI 950 system has been
used for studying the local viscoelastic properties of porcine
intervertebral disc end plate by means of nanoscale mechanical
dynamic analysis. The specimen of an endplate was cut from fresh
porcine vertebra dissected from 16 month animal. The lumbar spine
motion segments were dissected and 5 millimeter thick plates of
vertebral body, endplate and annulus fibrosus were prepared for
nanoindentation. The surface of the sample was kept in physiological
solution during nanoindentation experiment. We obtained mechanical
characteristics of different areas of native endplate (endplate middle
and vertebra and annulus fibrosus boundary).
Abstract: In this study, mechanically alloyed Al 2024 powder is
densified by conventional sintering and by equal channel angular
pressing (ECAP) with and without back pressure. The powder was
encapsulated in an aluminium can for consolidation through ECAP.
The properties obtained in the compacts by conventional sintering
route and by ECAP are compared. The effect of conventional
sintering and ECAP on consolidation behaviour of powder,
microstructure, density and hardness is discussed. Room temperature
back pressure aided ECAP results in nearly full denser (97% of its
theoretical density) compact at room temperature. NanoIndentation
technique was used to determine the modulus of the consolidated
compacts.