Abstract: An ordered porous antimony-doped tin oxide (ATO) film was successfully prepared using a simple coating process with colloidal templates. The facile production was effective when a combination of 16-nm ATO (as a model of an inorganic nanoparticle) and polystyrene (PS) spheres (as a model of the template) weresimply coated to produce a composite ATO/PS film. Heat treatment was then used to remove the PS and produce the porous film. The porous film with a spherical pore shape and a highly ordered porous structure could be obtained. A potential way for the control of pore size could be also achieved by changing initial template size. The theoretical explanation and mechanism of porous formation were also added, which would be important for the scaling-up prediction and estimation.
Abstract: Antimosy-doped tin oxide (ATO) particles were
prepared via chemical coprecipitation and reverse emulsion. The size
and size distribution of ATO particles were obviously decreased via
reverse microemulsion method. At the relatively high yield the ATO
particles were nearly spherical in shape, meanwhile the crystalline
structure and excellent conductivity were reserved, which could satisfy
the requirement as composite fillers, such as dielectric filler of
polyimide film.