In parallel, broadcasting has changed rapidly with the changing of the world at the same area. Broadcasting is also influenced and reshaped in terms of the emergence of new communication technologies. These developments have resulted a lot of economic and social consequences. The most important consequences of these results are those of the powers of the governments to control over the means of communication and control mechanisms related to the descriptions of the new issues. For this purpose, autonomous and independent regulatory bodies have been established by the state. One of these regulatory bodies is the Radio and Television Supreme Council, which to be established in 1994, with the Code no 3984. Today’s Radio and Television Supreme Council which is responsible for the regulation of the radio and television broadcasts all across Turkey has an important and effective position as autonomous and independent regulatory body. The Radio and Television Supreme Council acts as being a remarkable organizer for a sensitive area of radio and television broadcasting on one hand, and the area of democratic, liberal and keep in mind the concept of the public interest by putting certain principles for the functioning of the Board control, in the context of media policy as one of the central organs, on the other hand. In this study, the role of the Radio and Television Supreme Council is examined in accordance with the Code no 3894 in order to control over the communication and control mechanisms as well as the examination of the changes in the duties of the Code No. 6112, dated 2011.

Mechanical Properties of Particle Boards from Maize Cob and Urea-Formaldehyde Resin

Particle boards were prepared from Maize cob (MC) and urea-formaldehyde resin (UFR) on compression moulding machine. The amount of MC was varied from 50-120g while 30g of UFR was kept constant. Some mechanical properties of the particle boards were tested using the standard ASM methods. The results show that as the MC content increased from 50- 120g in 30g UFR, the hardness increased from about 6.89 x 102 to7.51 x 102MPa. Impact strength decreased from 3.3x 10-2 to 0.45 x 10-2J/M2, while tensile strength initially increased from 2.63 x 102 to 3.14 x 102 MPa as the MC increased from 50 to 60g in 30g UFR, thereafter, it decreased to about 1.35 x 102MPa at 120g in 30g content.