Abstract: The recycling process of Tungsten alloy (Swarf) by
oxidation reduction technique have been investigated. The reduced
powder was pressed under a pressure 20Kg/cm2 and sintered at
1150°C in dry hydrogen atmosphere. The particle size of the recycled
alloy powder was 1-3 μm and the shape was regular at a reduction
temperature 800°C. The chemical composition of the recycled alloy
is the same as the primary Swarf.