Volume:8, Issue: 12, 2014 Page No: 1317 - 1320
ISSN: 2415-6620
Stress Corrosion Crack (SCC) in pipeline is a type of
environmentally assisted cracking (EAC), since its discovery in 1965
as a possible cause of failure in pipeline, SCC has caused, on
average, one of two failures per year in the U.S, According to the
NACE SCC DA a pipe line segment is considered susceptible to SCC
if all of the following factors are met: The operating stress exceeds
60% of specified minimum yield strength (SMYS), the operating
temperature exceeds 38°C, the segment is less than 32 km
downstream from a compressor station, the age of the pipeline is
greater than 10 years and the coating type is other than Fusion
Bonded Epoxy(FBE). In this paper as a practical experience in
NISOC, Direct Assessment (DA) Method is used for identification
SCC defect in unpiggable pipeline located downstream of
compressor station.