Abstract: There is not much effective guideline on development of design parameters selection on spring back for advanced high strength steel sheet metal in U-channel process during cold forming process. This paper presents the development of predictive model for spring back in U-channel process on advanced high strength steel sheet employing Response Surface Methodology (RSM). The experimental was performed on dual phase steel sheet, DP590 in Uchannel forming process while design of experiment (DoE) approach was used to investigates the effects of four factors namely blank holder force (BHF), clearance (C) and punch travel (Tp) and rolling direction (R) were used as input parameters using two level values by applying Full Factorial design (24 ). From a statistical analysis of variant (ANOVA), result showed that blank holder force (BHF), clearance (C) and punch travel (Tp) displayed significant effect on spring back of flange angle (β2 ) and wall opening angle (β1 ), while rolling direction (R) factor is insignificant. The significant parameters are optimized in order to reduce the spring back behavior using Central Composite Design (CCD) in RSM and the optimum parameters were determined. A regression model for spring back was developed. The effect of individual parameters and their response was also evaluated. The results obtained from optimum model are in agreement with the experimental values.
Abstract: The objective of this project is to study the corrosion
behaviour and hardness based on the presence of martensite in dual
phase steel. This study was conducted on six samples of dual phase
steel which have different percentage of martensite. A total of 9
specimens were prepared by intercritical annealing process to study
the effect of temperature to the formation of martensite. The low
carbon steels specimens were heated for 25 minutes in a specified
temperature ranging from 7250C to 8250C followed by rapid cooling
in water. The measurement of corrosion rate was done by using
extrapolation tafel method, while potentiostat was used to control and
measured the current produced. This measurement is performed
through a system named CMS105. The result shows that a specimen
with higher percentage of martensite is likely to corrode faster.
Hardness test for each specimen was conducted to compare its
hardness with low carbon steel. The results obtained indicate that the
specimen hardness is proportional to the amount of martensite in dual
phase steel.
Abstract: In this study acoustic emission (AE) signals obtained during deformation and fracture of two types of ferrite-martensite dual phase steels (DPS) specimens have been analyzed in frequency domain. For this reason two low carbon steels with various amounts of carbon were chosen, and intercritically heat treated. In the introduced method, identifying the mechanisms of failure in the various phases of DPS is done. For this aim, AE monitoring has been used during tensile test of several DPS with various volume fraction of the martensite (VM) and attempted to relate the AE signals and failure mechanisms in these steels. Different signals, which referred to 2-3 micro-mechanisms of failure due to amount of carbon and also VM have been seen. By Fast Fourier Transformation (FFT) of signals in distinct locations, an excellent relationship between peak frequencies in these areas and micro-mechanisms of failure were seen. The results were verified by microscopic observations (SEM).
Abstract: Dual phase steels (DPS)s have a microstructure
consisting of a hard second phase called Martensite in the soft Ferrite
matrix. In recent years, there has been interest in dual-phase steels,
because the application of these materials has made significant usage;
particularly in the automotive sector Composite microstructure of
(DPS)s exhibit interesting characteristic mechanical properties such
as continuous yielding, low yield stress to tensile strength
ratios(YS/UTS), and relatively high formability; which offer
advantages compared with conventional high strength low alloy
steels(HSLAS). The research dealt with the characterization of
damage in (DPS)s. In this study by review the mechanisms of failure
due to volume fraction of martensite second phase; a new method is
introduced to identifying the mechanisms of failure in the various
phases of these types of steels. In this method the acoustic emission
(AE) technique was used to detect damage progression. These failure
mechanisms consist of Ferrite-Martensite interface decohesion and/or
martensite phase fracture. For this aim, dual phase steels with
different volume fraction of martensite second phase has provided by
various heat treatment methods on a low carbon steel (0.1% C), and
then AE monitoring is used during tensile test of these DPSs. From
AE measurements and an energy ratio curve elaborated from the
value of AE energy (it was obtained as the ratio between the strain
energy to the acoustic energy), that allows detecting important
events, corresponding to the sudden drops. These AE signals events
associated with various failure mechanisms are classified for ferrite
and (DPS)s with various amount of Vm and different martensite
morphology. It is found that AE energy increase with increasing Vm.
This increasing of AE energy is because of more contribution of
martensite fracture in the failure of samples with higher Vm. Final
results show a good relationship between the AE signals and the
mechanisms of failure.