Abstract: Spent petroleum catalyst from Korean petrochemical
industry contains trace amount of metals such as Ni, V and Mo.
Therefore an attempt was made to recover those trace metal using
bioleaching process. Different leaching parameters such as Fe(II)
concentration, pulp density, pH, temperature and particle size of
spent catalyst particle were studied to evaluate their effects on the
leaching efficiency. All the three metal ions like Ni, V and Mo
followed dual kinetics, i.e., initial faster followed by slower rate. The
percentage of leaching efficiency of Ni and V were higher than Mo.
The leaching process followed a diffusion controlled model and the
product layer was observed to be impervious due to formation of
ammonium jarosite (NH4)Fe3(SO4)2(OH)6. In addition, the lower
leaching efficiency of Mo was observed due to a hydrophobic coating
of elemental sulfur over Mo matrix in the spent catalyst.